This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2023, 14, 1085–1092, doi:10.3762/bjnano.14.89
Figure 1: Dependence of SnO2 film GPC on the evaporation temperature of the SnI4 precursor. The cycle times w...
Figure 2: Time evolution of the QCM mass sensor signal during five sequential ALD cycles (a), and during one ...
Figure 3: QCM frequency decrement measured per single ALD cycle as function of the SnI4 pulse length. The len...
Figure 4: SnO2 film GPC as function of the number of ALD cycles.
Figure 5: SnO2 GPC as function of the substrate temperature.
Figure 6: Oxygen content in the SnO2 films as function of the substrate temperature.
Figure 7: Content of residual iodine in tin oxide films deposited from tin iodide and ozone in the temperatur...
Figure 8: GIXRD patterns of SnO2 films deposited at the given temperatures. Miller indices attributed to the ...
Figure 9: Refractive index of a SnO2 film deposited at 300 °C to a thickness of 110 nm as function of the wav...
Figure 10: XPS results of (a) Sn 3d, (b) O 1s, and (c) valence-band region of the SnO2 films deposited at 300 ...
Figure 11: XAS results depicting O 1s (a) and Sn 3d (b) spectra of the SnO2 films deposited at 300 and 500 °C.
Beilstein J. Nanotechnol. 2018, 9, 119–128, doi:10.3762/bjnano.9.14
Figure 1: Growth rates of Fe2O3, ZrO2 and their mixtures with different cycle ratios as a function of sample ...
Figure 2: Grazing incidence X-ray diffraction (XRD) patterns for ZrO2/Fe2O3 films deposited on TiN with ZrO2/...
Figure 3: Grazing incidence X-ray diffraction (XRD) patterns for ZrO2/Fe2O3 films deposited on Si(100) with Z...
Figure 4: SEM image of a ZrO2/Fe2O3 film grown in a 3D stacked structure (left panel) and images of ZrO2/Fe2O3...
Figure 5: TEM image of a ZrO2/Fe2O3 sample with cycle ratio 10:3 on TiN. 231 atomic layer deposition cycles w...
Figure 6: Each of the three panels show a sensed voltage–applied voltage curve on the left (a) and a polariza...
Figure 7: Current density–applied electric field curves for samples with ZrO2/Fe2O3 cycle ratios shown in the...
Figure 8: Selected room temperature magnetization–field curves for ZrO2/Fe2O3 films. Cycle ratios and thickne...
Beilstein J. Nanotechnol. 2017, 8, 229–236, doi:10.3762/bjnano.8.25
Figure 1: Construction of the flow cell for reflectance measurements.
Figure 2: Working principle of the sensor element: the light reflected from the surface of the film and from ...
Figure 3: Characterization of the synthesized NPs and their thin films bound with PTSA. (a) TEM images of TiO2...
Figure 4: (a) UV–vis reflectance spectra of the film exposed to different ethanol concentrations and cleaned ...
Figure 5: Left: schematic diagram of height profile measurements before and after absorption of ethanol. Righ...
Figure 6: Optical response of the TiO2 NP-based thin film towards different VOCs (i.e., dependence of the shi...